SAND SAND SAND SAND...I can't stress that enough. You want to take the case down to the metal (assuming you're talking about a case here...even if you aren't, SAND!). Then prime the surface, then sand some more. Prime again, sand again. Actually, here...
http://deron.meranda.us/casemod/painting/
Those steps can be used for plastics as well...just remember to use that Krylon Fusion stuff...it REALLY works well (I've used it several times). |
|